Laboratory Test Sheet
                                        HOT SAND TEST BITUMINOUS PAVEMENT MATERIALS
Client :
Alfred McAlpine Civil Engineering
Site :
Stanton North Phase II
Client Ref :
12345
10073
Job No :
B4240/96V
Date Received :
04/09/1996
LabRef :
Supplier :
Source :
Material Type :
Type 1 Sub-base
Specification :
Sub-base
Material Name :
Binder Type/Grade :
Type 1 Sub-base
          Sand Preparation
          Spread 150-300um sand 25mm deep on                                                  Time in
          two trays.  Place in oven at 125 to 130C                                                  Time out
          for at least 2 hours.
               Sieve Chippings for 30 Seconds
          Use a 10mm sieve for 20mm Chips or a
          6.3mm sieve for 14mm Chips.
          Moisture on Pre-Coated Chippings
          If wet then place in Oven for at least                                                       Time in
          2 hours at 60C.                                                                           Time out
          Weight of Dried Sample                                                                 W1(g)
          Check Sand Temperatures
          Check at several points in the tray
          If 125 to 130C has not been reached
          leave for a further period.
          Spread Chippings
          Place Chippings in Hot Sand within
          2 to 3 minutesto prevent heat loss.
          Check Final Sand Temperature>100
          After placing Chippings in the Oven for a                                                  Time in
          minimum of 10 minutesCheck final Sand                                                  Time out
          Temperature>100C
          Remove Chippings
          Pour onto a 3.35mm Sieve and allow to cool                                                  C
          for about 10 minutes
          Place in Tin
          Place in the 4.5 litre Tin with the 1.18 to 600
          grit and attach lid
          Shake in Tin
          Shake Tin longitudinally a total of 100 cycles
          in about 50 secondswith a displacement of
          about 100mm
          Wash Chippings
          Pour Chippings and Sand onto a 3.35mm Sieve.
          Disgard Sandand wash Chipsplace
          on absorbent paper and dry with Hot air blower
          Weight of Dried Treated Sample
          Report to nearest 0.1g                                                                           W2(g)
          Sand Retention
          Report to nearest 0.1g/kg                         (W1-W2)/W1 * 1000                         g/kg
          Weight of Rejected Sample
          Chips with less than half Sand cover                                                            W3(g)
          Proportion of Rejected Chips
          Report to nearest 0.1%                              (W3 * 100)/W2                              %
Comments :
Tested By :                                        Date :                         Checked By :                                   Date :
                                                                                Check Level (1/2/3)
Notes :          Delete as applicable